STRESS UNIT CONVERTER
| kPa | Pa = N/m² | gf/cm² | kgf/m² | bar | PSI | |
| 1 kPa ( kilopascal ) | = 1 | = 1000 | = 10.197 | = 101.97 | = 0.01 | = 0.145 |
| 1 Pa (pascal) | = 0.001 | = 1 | = 0,010197 | = 0,10197 | = 1.0E-5 |
= 0,000145038 |
| 1 N/m² | = 0.001 | = 1 | = 0,010197 | = 0,10197 | = 1.0E-5 | = 0,000145038 |
| 1 gf/cm² | = 0,098 | = 98,0665 | = 1 | = 10 | = 0,000981 | = 0,014223369 |
| 1 kgf/m² | = 0,0098 | = 9,80665 | = 0,1 | = 1 | = 9.80665E-5 |
= 0,0014223369 |
| 1 bar | = 100 | = 100000 | = 1019,716 | = 10197,16 | = 1 | = 14,5038 |
| 1 PSI | = 6,8947 | = 6894,74 | = 70,30683 | = 703,068 | = 0,068947 | = 1 |